Naturally Hard Copper Alloys

780 bytes removed, 09:54, 4 January 2023
Copper-Tin Alloys (Tin Bronze)
</figtable>
<sup>1)</sup> t: Strip thickness max. 0.5 mm
 
<xr id="fig:Softening of CuZn36 50"/><!--Fig. 5.9:--> Softening of CuZn36 after 3 hrs annealing after 50% cold working)
 
<xr id="fig:Phase diagram of the Cu-Sn system for the range of 0 – 30 wt% Sn"/><!--Fig. 5.10:--> Phase diagram of the Cu-Sn system for the range of 0 – 30 wt% Sn)
 
<xr id="fig:Mechanical properties of tin bronze depending on the tin content (cold working 0 and 50%)"/><!--Fig. 5.11:--> Mechanical properties of tin bronze depending on the tin content (cold working 0 and 50%)
 
<xr id="fig:Strain hardening of CuSn8 by cold working"/><!--Fig. 5.12:--> Strain hardening of CuSn8 by cold working
 
<xr id="fig:Softening of CuSn8 after 3 hrs annealing after 50% cold working"/><!--Fig. 5.13:--> Softening of CuSn8 after 3 hrs annealing after 50% cold working