6.4.4 Switching Contacts
<xr id="fig:fig6.9"/> Fig. 6.9: Histogram of the contact resistance Rk of an electroplated palladium layer (3 μm) with and without hard gold flash plating (0.2 μm) after exposure with different plastic materials
 
<xr id="fig:fig6.10"/> Fig. 6.10: Contact resistance with exposure to out gasing from plastics
 
<div class="multiple-images">
<figure id="fig:fig6.9">
[[File:Histogram of the contact resistance Rk.jpg|left|thumb|<caption>Histogram of the contact resistance R<sub>K< /sub> of an electroplated palladium layer (3 μm) with and without hard gold flash plating (0.2 μm) after exposure with different plastic materials</caption>]]
</figure>
 
<figure id="fig:fig6.10">
[[File:Contact resistance with exposure to out gasing from plastics.jpg|left|thumb|<caption>Contact resistance with exposure to out-gasing from plastics as a function of numbers of operations at 6 V<sub>DC</sub>,100 mA: 1 Silicon containing plastic; 2 Plastics with strongly out-gasing components; 3 Plastics with minimal out-gasing components</caption>]]