*'''Influence of out-gasing from plastics'''
 <xr id="fig:fig6.9"/> Fig. 6.9:Histogram of the contact resistance Rk of an electroplated palladium layer (3 μm) with and without hard gold flash plating (0.2 μm) after exposure with different plastic materials <div class="multiple-images"><figure id="fig:fig6.9">[[File:Histogram of the contact resistance Rk.jpg|left|thumb|<caption>Histogram of the contactresistance R <sub>K< /sub> of an electroplated Kpalladium layer (3 μm) with andwithout hard gold flash plating(0.2 μm) after exposure withdifferent plastic materials</caption>]]</figure></div><div class="clear"></div>
Fig. 6.10: Contact resistance with exposure to out-gasing from plastics as a function of numbers of