5.1.4.2 Copper-Tin Alloys (Tin Bronze)
behavior are shown for the example of CuSn8 in <xr id="fig:Strain hardening of CuSn8 by cold working"/> Figures 5.12 and <xr id="fig:Softening of CuSn8 after 3 hrs annealing after 50% cold working"/> 5.13. The stress relaxation properties for CuSn alloys are good for up to 100°C, deteriorate however quickly for temperatures above 150°C.
Fig. 5.9: Softening of CuZn36 after 3 hrs annealing after 50% cold working(im Text nicht zu finden!)
[[File:Softening of CuZn36 50.jpg|right|thumb|Softening of CuZn36 after 3 hrs annealing after 50% cold working]]