6.4.4 Switching Contacts
**'''Arc erosion'''
<xr id="fig:fig6.13"/> Fig. 6.13 : Arc erosion of a Ag/SnO<sub>2</sub> contact pair after extreme arcing conditionsa) Overall view; b) Partial detail view <div class="multiple-images"><figure id="fig:fig6.13">[[File:Arc erosion of a AgSnO2 contact pair after extreme arcing conditions.jpg|left|thumb|<caption>Arc erosion of a Ag/SnO<sub>2</sub> contact pair after extreme arcing conditions a) Overall view; b) Partial detail view</caption>]]</figure></div><div class="clear"></div>
**'''Contact welding'''