5.1.5.2 Copper-Nickel-Tin Alloys
Fig. 5.24: Strain hardening of CuNi25 by cold working
[[File:Strain hardening of CuNi25 by cold working.jpg|right|thumb|Strain hardening of CuNi25 by cold working]]
Fig. 5.25: Softening of CuNi25 after 1 hr annealing after 50% cold working