Difference between revisions of "Template:MainPicture"

From Electrical Contacts
Jump to: navigation, search
 
(13 intermediate revisions by the same user not shown)
Line 1: Line 1:
<div class=picture-item clear>
+
<div class="picture-item">
<randomimage size="170px" float="left" choices="SofteningOfCuETPafterAnnealing.png|Strain_hardering.png" />
+
<rimage size="170px" float="left" info="1" />
<div class=picture-item-text style="float:left; padding-top: 5px"> Different shapes of silver powders <br>
+
 
at:  [[Carrier Materials]] by [[Musteruser]]
+
</div>
Categories: [[Metal Powders]], [[Metal Firing Preparations]]</div></div><br>
+
<div style="clear:both"></div>
<div class=picture-item>
+
<div class="picture-item">
<randomimage size="170px" float="left" choices="Qualitaetsmerkmale und Toleranzen.jpg |Dimensional Ranges.jpg |Ty pical Contact Shapes of Solid Contact Rivets.jpg" />
+
<rimage size="170px" float="left" info="1" />
<div class=picture-item-text style="float:left;padding-top: 5px"> Different shapes of silver powders <br>
+
</div>
at:  [[Carrier Materials]] by [[Musteruser]]
 
Categories: [[Metal Powders]], [[Metal Firing Preparations]]</div></div><br>
 

Latest revision as of 13:43, 6 May 2014

Micro structure of Ag ZnO 92 8 WPW25.jpg
Micro structure of Ag/ZnO 92/8 WPW25:a) perpendicular to extrusion direction b) parallel to extrusion direction, 1) Ag/ZnO contact layer, 2) Ag backing layer
Pages: Silver Based Materials,
Werkstoffe auf Silber-Basis

by Doduco Redaktion


Softening of AgCdO9010P after annealing.jpg
Softening of Ag/CdO 90/10 P after annealing for 1 hr after 40% cold working