Silver-Palladium Alloys
'''Table 2.18: Mechanical Properties of Silver-Palladium Alloys'''
<table class="twocolortable">
<tr><th><p class="s12">Material</p></th><th><p class="s12">Hardness</p><p class="s12">Condition</p></th><th><p class="s12">Tensile Strength</p><p class="s12">R<span class="s31"><sub>m </sub></span>[MPa]</p></th><th><p class="s12">Elongation A</p><p class="s12">[%]min.</p></th><th><p class="s12">Vickers Hardness</p><p class="s12">HV</p></th></tr><tr><td><p class="s12">AgPd30</p></td><td><p class="s12">R 320</p><p class="s12">R 570</p></td><td><p class="s12">320</p><p class="s12">570</p></td><td><p class="s12">38</p><p class="s12">3</p></td><td><p class="s12">65</p><p class="s12">145</p></td></tr><tr><td><p class="s12">AgPd40</p></td><td><p class="s12">R 350</p><p class="s12">R 630</p></td><td><p class="s12">350</p><p class="s12">630</p></td><td><p class="s12">38</p><p class="s12">2</p></td><td><p class="s12">72</p><p class="s12">165</p></td></tr><tr><td><p class="s12">AgPd50</p></td><td><p class="s12">R 340</p><p class="s12">R 630</p></td><td><p class="s12">340</p><p class="s12">630</p></td><td><p class="s12">35</p><p class="s12">2</p></td><td><p class="s12">78</p><p class="s12">185</p></td></tr><tr><td><p class="s12">AgPd60</p></td><td><p class="s12">R 430</p><p class="s12">R 700</p></td><td><p class="s12">430</p><p class="s12">700</p></td><td><p class="s12">30</p><p class="s12">2</p></td><td><p class="s12">85</p><p class="s12">195</p></td></tr><tr><td><p class="s12">AgPd30Cu5</p></td><td><p class="s12">R 410</p><p class="s12">R 620</p></td><td><p class="s12">410</p><p class="s12">620</p></td><td><p class="s12">40</p><p class="s12">2</p></td><td><p class="s12">90</p><p class="s12">190</p></td></tr></table>
</figtable>