→5.1.2 Pure Copper
</figtable>
<xr id="fig:fig5.1"/> Fig. 5.1: Strain hardening of Cu-ETP by cold working <xr id="fig:fig5.2"/> Fig. 5.2: Softening of Cu-ETP after annealing for 3hrs after 25% cold working <xr id="fig:fig5.3"/> Fig. 5.3: Softening of Cu-ETP after annealing for 3hrs after 50% cold working <div class="multiple-images"> <xr id="fig:fig5.1"/>
[[File:Strain hardening of Cu ETP by cold working.jpg|right|thumb|Strain hardening of Cu-ETP by cold working]]
[[File:Softening of Cu ETP after annealing.jpg|right|thumb|Softening of Cu-ETP after annealing for 3hrs after 25% cold working]]
</figure>
<figure id="fig:fig5.3">
[[File:Softening of Cu ETP after annealing 50.jpg|right|thumb|Softening of Cu-ETP after annealing for 3hrs after 50% cold working]]
</figure>
</div>
<div class="clear"></div>
===5.1.3 High Cu Content Copper Alloys===