Changes

AC-3 contact arc erosion of two differently produced Ag/SnO2 contact materials in a 37 kW contactor 1 Ag/SnO2 88/12, produced by conventional powder metallurgy with MoO3 additive, extruded 2 Ag/SnO2 88/12, powder manufacturing by the reaction-spray pro...
== Summary ==
AC-3 contact arc erosion of two differently produced Ag/SnO2 contact materials
in a 37 kW contactor
1 Ag/SnO2 88/12, produced by conventional
powder metallurgy with MoO3 additive,
extruded
2 Ag/SnO2 88/12, powder manufacturing by
the reaction-spray process with CuO and Bi2O3 additives, extruded