Brazed Joints
=== Brazed Joints===
Despite optimized brazing parameters non-wetted defect areas in the braze joint cannot be avoided completely. These wetting defects can mostly be traced to voids caused by flux inclusions in the braze joint area. Depending on the shape and size of the joint areas, the portion of the fully wetted joint is between 65% and 90%. In its final use in switching devices a joint area of 80% is considered good or excellent if the individual void size does not exceed 5% of the joint area. Frequently wetted joint areas >90% with voids <3% can be obtained.
Evaluation of the quality of the joint can be performed either by destructive or non-destructive methods.