File:Softening of AuAg20Cu10 after annealing for 0.5 hrs.jpg
Softening_of_AuAg20Cu10_after_annealing_for_0.5_hrs.jpg (368 × 270 pixels, file size: 34 KB, MIME type: image/jpeg)
Summary
Description | Softening of AuAg20Cu10 after annealing for 0.5 hrs after 80% cold working |