(AC-3 contact arc erosion of two differently produced Ag/SnO2 contact materials in a 37 kW contactor 1 Ag/SnO2 88/12, produced by conventional powder metallurgy with MoO3 additive, extruded 2 Ag/SnO2 88/12, powder manufacturing by the reaction-spray pro...) |
(No difference)
|
Revision as of 14:36, 23 April 2014
Summary
AC-3 contact arc erosion of two differently produced Ag/SnO2 contact materials in a 37 kW contactor 1 Ag/SnO2 88/12, produced by conventional powder metallurgy with MoO3 additive, extruded 2 Ag/SnO2 88/12, powder manufacturing by the reaction-spray process with CuO and Bi2O3 additives, extruded
Licensing
![]() |
Dieses Werk ist lizenziert unter einer Creative Commons Namensnennung-Nicht kommerziell 4.0 International Lizenz |
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 14:36, 23 April 2014 | ![]() | 309 × 348 (31 KB) | Doduco Redaktion (talk | contribs) | AC-3 contact arc erosion of two differently produced Ag/SnO2 contact materials in a 37 kW contactor 1 Ag/SnO2 88/12, produced by conventional powder metallurgy with MoO3 additive, extruded 2 Ag/SnO2 88/12, powder manufacturing by the reaction-spray pro... |
- You cannot overwrite this file.
File usage
The following 2 pages link to this file: