2,808
edits
Changes
no edit summary
[[File:Strain hardening of PdCu40 by cold working.jpg|right|thumb|Strain hardening of PdCu40 by cold working]]
Fig. 2.43: Softening of PdCu40 after annealing for 0.5 hrs after 80% cold working
[[File:Softening of PdCu40 after annealing.jpg|right|thumb|Softening of PdCu40 after annealing for 0.5 hrs after 80% cold working]]
Fig. 2.44: Electrical resistivity p of PdCu alloys with and without an annealing step for forming an ordered phase