2,808
edits
Changes
→5.1.5.2 Copper-Nickel-Tin Alloys
Fig. 5.27: Softening of CuNi9Sn2 after 1 hr annealing after 60% cold working (Wieland)
[[File:Softening of CuNi9Sn2 after annealing Wieland.jpg|right|thumb|Softening of CuNi9Sn2 after 1 hr annealing after 60% cold working (Wieland)]]