File:Softening of AuAg26Ni3 after annealing for 0.5-hrs.jpg

From Electrical Contacts
Revision as of 15:51, 16 December 2013 by Ermisch (talk | contribs) (Softening of AuAg26Ni3 after annealing for 0.5 hrs after 80% cold working)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to: navigation, search
Softening_of_AuAg26Ni3_after_annealing_for_0.5-hrs.jpg(375 × 281 pixels, file size: 36 KB, MIME type: image/jpeg)

Summary

Description Softening of AuAg26Ni3 after annealing for 0.5 hrs after 80% cold working
Author Doduco Redaktion
Date

Licensing

Creative Commons Lizenzvertrag Dieses Werk ist lizenziert unter einer Creative Commons Namensnennung-Nicht kommerziell 4.0 International Lizenz

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current15:51, 16 December 2013Thumbnail for version as of 15:51, 16 December 2013375 × 281 (36 KB)Doduco Redaktion (talk | contribs)Softening of AuAg26Ni3 after annealing for 0.5 hrs after 80% cold working
  • You cannot overwrite this file.

The following 2 pages link to this file: