Open main menu

Electrical Contacts β

File:Softening of AuAg20Cu10 after annealing for 0.5 hrs.jpg

Softening_of_AuAg20Cu10_after_annealing_for_0.5_hrs.jpg(368 × 270 pixels, file size: 34 KB, MIME type: image/jpeg)

Summary

Description Softening of AuAg20Cu10 after annealing for 0.5 hrs after 80% cold working
Author Doduco Redaktion
Date

Licensing

Creative Commons Lizenzvertrag Dieses Werk ist lizenziert unter einer Creative Commons Namensnennung-Nicht kommerziell 4.0 International Lizenz

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current15:56, 16 December 2013Thumbnail for version as of 15:56, 16 December 2013368 × 270 (34 KB)Doduco Redaktion (talk | contribs)Softening of AuAg20Cu10 after annealing for 0.5 hrs after 80% cold working