{||-|Description|Frequency distribution of the contact resistance of a contaminated contact surface (Ag rivet with electroplated hard gold layer; test parameters: 10 mV, 10 mA, 10 cN)|-|Author |Doduco Admin|-|Date|16.04.2014|}