Fluxes
the brazing surfaces and prevent their new build-up in order to allow a thorough wetting of these surfaces by the liquefied brazing alloy. Fluxes have to be activated already at a temperature below the working range of the brazing alloy. They are selected mainly according to the working temperature of the brazing alloy and the base material to be joined.
Tab 4.1Commonly Used Brazing Alloys for Electrical Contacts
[[File:Commonly Used Brazing Alloys for Electrical Contacts.jpg|right|thumb|Commonly Used Brazing Alloys for Electrical Contacts]]