→5.2.2 Nickel Alloys
Fig. 5.48: Softening of NiCu30Fe after annealing for 0.5 hrs and after 80% cold working
[[File:Softening of NiCu30Fe after annealing for 0.5 hrs.jpg|right|thumb|Softening of NiCu30Fe after annealing for 0.5 hrs and after 80% cold working]]
'''Table 5.21: Physical Properties of Nickel and Nickel Alloys''' (2 Teile!)