Softening of CuAg2 after 1 hr annealing after 80% cold working
== Summary ==
{|
|-
|Description
|Softening of CuAg2 after 1 hr annealing after 80% cold working
|-
|Author
|Doduco Redaktion
|-
|Date
|
|}
== Licensing =={{CC-by-sa-4.0}}
{|
|-
|Description
|Softening of CuAg2 after 1 hr annealing after 80% cold working
|-